Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1310 MPa | 190000 psi | |
Kinetics MIM 4605 Low Alloy Steel (Quenched + Tempered) Low alloy steel, carbon, nickel, molybdenum. A multi-purpose, economical material that offers various strength, hardness, and wear resistance properties depending if it is heat treated and the heat .. |
|||
Tensile Strength, Yield | 1310 - 1340 MPa @Strain 0.200 % |
190000 - 194000 psi @Strain 0.200 % |
|
Latrobe Lescalloy® HP 9-4-30 VAC-ARC ; 5.75 in RCS Billet Size High Strength Alloy Steel LESCALLOY HP 9-4-30 VAC-ARC steel is a low alloy, high strength steel with a high nickel and cobalt content to promote toughness. The alloy has been designed to have high hardenability, good weldabi.. |
|||
Tensile Strength, Yield | 1310 MPa @Temperature 23.0 °C |
190000 psi @Temperature 73.4 °F |
0° |
Hexcel® HexPly® 954-3 Curing Cyanate Resin, K1100 Fiber Information provided by HexCel |
|||
Tensile Strength, Yield | 1310 MPa | 190000 psi | |
Elgiloy® Co-Cr-Ni Alloy, Strip, 50% Cold Reduction The strength, elongation, and hardness values are specific to this cold reduction treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, ductility, fati.. |
|||
Tensile Strength, Yield | 1310 MPa | 190000 psi | |
Elgiloy® Co-Cr-Ni Alloy, Wire, 40% Cold Reduction The strength, shear modulus, and hardness values are specific to this cold reduction treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, ductility, f.. |
|||
Tensile Strength, Yield | 1310 MPa @Strain 0.200 % |
190000 psi @Strain 0.200 % |
|
AK Steel 17-7 PH® Precipitation Hardening Stainless Steel, Condition C AK Steel 17-7 PH® provides high strength and hardness, excellent fatigue properties, good corrosion resistance, good formability, and minimum distortion upon heat treatment. This alloy provides va.. |
|||
Tensile Strength, Yield | 1310 MPa @Strain 0.200 % |
190000 psi @Strain 0.200 % |
|
AK Steel PH 15-7 Mo® Precipitation Hardening Stainless Steel, Condition C AK Steel 15-7 Mo® provides high strength and hardness, good corrosion resistance and minimum distortion on heat treatment. It is easily formed in the annealed condition and develops effective bala.. |
|||
Tensile Strength, Yield | 1310 MPa @Strain 0.200 %, Temperature 149 °C |
190000 psi @Strain 0.200 %, Temperature 300 °F |
|
Carpenter MP35N* Ni-Co-Cr-Mo Alloy, Cold Drawn 33%, Aged 565°C/4hr/AC Data provided by Carpenter Technology Corporation.Carpenter MP35N alloy is a nonmagnetic, nickel-cobalt-chromium-molybdenum alloy possessing a unique combination of ultrahigh tensile strength, good .. |
|||
Tensile Strength, Yield | 1310 MPa @Strain 0.200 % |
190000 psi @Strain 0.200 % |
|
ATI Allegheny Ludlum AL 13-8™ H 1000 Precipitation Hardening Alloy Characteristics: excellent strength, high hardness, superior toughness, good corrosion resistance, good transverse toughness properties, strength and ductility can be tailored by varying the aging t.. |