Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 12.35 - 13.65 MPa | 1791 - 1980 psi | ±5% change after 70 hours @ 100°C; ASTM D412 |
Precision Polymer Engineering N70M Nitrile Rubber Nitrile Butadiene Rubber (NBR), 68-78 °IRHD. Copolymer of acrylonitrile and butadiene. To meet BS2751 BA70 and ASTM D2000/SAE J200 line call-out 2MBG 714, B14, EA14, EF11, EF21, EO14, EO34, F17.Ap.. |