Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 13.11 MPa | 1902 psi | ASTM D638 |
Reltek BONDiTâ„¢ B-52 Adhesive, Sealant & Potting System Key Properties: Outstanding for bonding dissimilar materials with high thermal expansion differential applications.Fast thermal cure, long pot life.Ease of use.Applications: Excellent for fast assem.. |