Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 67.0 - 128 MPa | 9720 - 18500 psi | Average value: 90.0 MPa Grade Count:36 |
Overview of materials for Nylon 66, 40% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Mineral Filled". Specific grades with primary filler content between 35% and 44% are inclu.. |