Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 127.6 MPa @Thickness 3.17 mm |
18510 psi @Thickness 0.125 in |
ASTM D638 |
PTS Tristar® PC-30GF 30% Glass Reinforced Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |