Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 8.69 MPa | 1260 psi | ASTM D412 |
Polymax® Maxelast® C4750 TPE, Transparent Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsWire & Cable ElectronicsMedical DevicesPlastic TougheningInf.. |
|||
Tensile Strength, Yield | 8.70 MPa | 1260 psi | ASTM D412 |
Precision Polymer Engineering Perlast® G50S FFKM White Perfluoroelastomer Perlast® G50S FFKM is a White Perfluoroelastomer 50-55 °IRHD. It has excellent chemical resistance, steam resistance and mechanical properties. Suitable for use in all food applications, and extr.. |
|||
Tensile Strength, Yield | 8.69 MPa | 1260 psi | Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412 |
PolyOne Synprene® RT-3975 Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:High Performance Thermoplastic ElastomerUV StabilizedNaturalApplications:Multi-PurposeMarket:AutomotiveBuilding and ConstructionConsumer GoodsIndustrialProcessing Method:Injecti.. |