Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 85.15 MPa | 12350 psi | ASTM D638 |
Nilit Polynil® P50FL Externally Lubricated, Lightly Nucleated Nylon 66 Description: Polynil P50FL is a general purpose injection molding grade that is widely used for gears, bearings, fasteners, clips.Key characteristics: Excellent flowGood toughnessGood overall mechan.. |