Mechanical Properties Metric English Comments
Tensile Strength, Yield 1230 MPa

@Strain 0.200 %
178000 psi

@Strain 0.200 %
Haynes 625 alloy, 40% cold reduction
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of hi..