Mechanical Properties Metric English Comments
Tensile Strength, Yield 12.68 MPa
1839 psi
-0.5% change after 168 hours @ 70°C; ASTM D412
Precision Polymer Engineering C40M Chloroprene Rubber
Chloroprene elastomer, 36-45 °IRHD. Formulated to BS 2752 grade C40.Applications: A versatile rubber with good compression set properties, giving moderate resistance to petroleum based oils, ozone ..