Polymer Property : Tensile Strength, Yield = 12.56 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 12.56 MPa
1822 psi
AVG Stress at Elongation M25; ASTM D412 Method A
Seals Eastern 7182A Fluorocarbon-Elastomer
Formulated AFLAS® high-temperature, high-pressure "sour" oil & gas service. Resistant to extrusion. Excellent acid and base resistance.Information provided by Seals Eastern, Inc.