Tensile Strength, Yield 81.98 MPa
11890 psi
ASTM D638
Aclo Accucomp Nylon 66 NY0750L
Tensile Strength, Yield 81.98 MPa
11890 psi
ASTM D638
Aclo Accutech ABS ABS833G20L Glass Reinforced
Tensile Strength, Yield 81.98 MPa
11890 psi
ASTM D638
Aclo Accutech Polypropylene Homopolymer HP0336G40CL Glass Reinforced Coupled