Polymer Property : Tensile Strength, Yield = 1175 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 8.102 MPa
1175 psi
96% Retention; Air Over Aged 400 hrs at 107°C
Teknor Apex TEKRON® 4300-D88A Thermoplastic Elastomer
Information provided by Teknor Apex Company