Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 0.793 MPa @Strain 300 % |
115 psi @Strain 300 % |
Method A (Dumbbell & Section), 20 in/min; ASTM D412 |
PolyOne Synprene® RT-3720 Thermoplastic Elastomer - SBC, Mineral Filled
(discontinued **) Description/Features:Multi-Purpose Thermoplastic ElastomerMineral FilledNaturalApplications:General PurposeMarket:Consumer GoodsIndustrialBuilding and ConstructionProcessing Method:Injection Molding.. |