Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1148 MPa @Strain 0.200 % |
166500 psi @Strain 0.200 % |
|
AK Steel 17-4 PH® Precipitation Hardening Stainless Steel, Condition H 1075 AK Steel 17-4 PH® provides an outstanding combination of high strength, good corrosion resistance, good mechanical properties at temperatures up to 600°F (316°C), and good toughness in both base.. |