Polymer Property : Tensile Strength, Yield = 1119 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 7.715 MPa
1119 psi
AVG Stress at Elongation M50; ASTM D412 Method A
Seals Eastern 7182E Fluorocarbon-Elastomer
Formulated AFLAS® high-temperature "sour" oil & gas service. Excellent acid and base resistance.Information provided by Seals Eastern, Inc.