Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 11.25 MPa | 1632 psi | 25% change after 168 hours @ 100°C; ASTM D412 |
Precision Polymer Engineering N70J Nitrile Rubber Peroxide cured Nitrile Butadiene Rubber (NBR), 66-75 °IRHD. Copolymer of acrylonitrile and butadiene. To meet DTD 5594A standard for resistance to mineral oils.Applications: Excellent resistance i.. |
|||
Tensile Strength, Yield | 11.25 MPa | 1632 psi | -25% change after 70 hours @ 150°C; ASTM D412 |
Precision Polymer Engineering Z75L Hydrogenated NBR Compound Peroxide Cured, Hydrogenated Nitrile Rubber, 75-85 °IRHD. Low acrylonitrile content (ACN = 17%).Applications: Specially compounded for service in low-temperature applications. High strength and ex.. |