Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Yield = 11.118 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 11.118 MPa
1612.5 psi
212°F, 70 hr, in IRM 903 Oil; ASTM D573
ExxonMobil Vyram™ 9103-54 Thermoplastic Elastomer  (discontinued **)
A hard, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing characteristi..
Tensile Strength, Yield 11.118 MPa
1612.5 psi
212°F, 70 hr, in IRM 903 Oil; ASTM D471
ExxonMobil Vyram™ 9203-54 Thermoplastic Elastomer  (discontinued **)
A hard, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing character..
Copyright © lookpolymers.com All Rights Reserved