Polymer Property : Tensile Strength, Yield = 1069 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 1069 MPa

@Strain 0.200 %
155000 psi

@Strain 0.200 %
ATI Allvac® Ti-17 Titanium Alloy, Heat Treatment: 899°C (1650°F) + Age
Data provided by Allvac.Applications: Compressor discs, heavy section forgings for gas turbine engine components. High tensile strength and good fracture toughness.
Tensile Strength, Yield 1069 MPa

@Strain 0.200 %
155000 psi

@Strain 0.200 %
ATI Allvac® Vasco® 15-5 Precipitation Hardening Steel, Heat Treatment: 1038°C (1900°F) + Age
Data provided by Allvac.Applications: Aircraft and missile fittings, fasteners, gears. Turbine and pump blades, shafts.
Tensile Strength, Yield 1069 MPa

@Strain 0.200 %
155000 psi

@Strain 0.200 %
ATI Allvac® Vasco® 17-4 Precipitation Hardening Steel, Heat Treatment: 1038°C (1900°F) + Age
Data provided by Allvac.Applications: Aircraft and missile fittings, fasteners, gears. Turbine and pump blades, shafts.
Tensile Strength, Yield 1069 MPa
155000 psi
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 302, 60% Cold Rolled (UNS S30200)
This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to ..
Tensile Strength, Yield 1069 MPa
155000 psi
HP Alloys Alloy 718, 25% Cold Worked
25% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internati..