Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1025 MPa @Strain 0.200 % |
148700 psi @Strain 0.200 % |
|
Haynes 214® alloy, 20% cold reduction Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Tensile Strength, Yield | 1025 MPa @Strain 0.200 % |
148700 psi @Strain 0.200 % |
|
Haynes 25 alloy, room temperature after 15% cold reduction Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal gall.. |