Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1024 MPa @Strain 0.200 % |
148500 psi @Strain 0.200 % |
|
Haynes R-41 alloy, 1.27 mm thick sheet, solution heat treated at 1079°C, water quenched, 30 minutes at 1066°C, aged 16 hours at 760°C (1400°F), air cooled Vacuum melted, exceptionally high strength at temperature between 649-982°C. Precipitation-hardening type, strength developed by various solutioning and aging heat treatments. Applications includ.. |
|||
Tensile Strength, Yield | 1024 MPa @Strain 0.200 % |
148500 psi @Strain 0.200 % |
|
Special Metals INCONEL® 706 Precipitation Hardening Alloy, Cold Rolled Sheet, 3 Part Heat Treatment, 0.040 inch (1.02 mm) Thickness Tensile strength (ultimate and yield), shear strength, and elongation values reported here are typical for Cold Rolled Sheet, 3 Part Heat Treatment, 0.040 inch (1.02 mm) Thickness samples. Density a.. |