Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1017 MPa @Temperature 23.0 °C |
147500 psi @Temperature 73.4 °F |
prEN2561 Type B |
Hexcel® HexPly® M35-4 80-180°C Curing Epoxy Matrix, M35-4/40%/G1089/1000 Fabric Fiber: T800H 6K 2x2 Twill, 200 g/m2Information provided by HexCel |