Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 696 MPa | 101000 psi | Hot-Worked |
Kinetics MIM F1537 (ASTM F1537) HIP and Heat Treat Most commonly used within the medical market on applications requiring these characteristics: Bio-compatibility Corrosion resistance High strength Nonmagnetic Wear resistance. Information prov.. |
|||
Tensile Strength, Yield | 696 - 827 MPa | 101000 - 120000 psi | 0.2% offset |
Eagle Brass 762 Nickel Silver 12%, Spring 762 is a nickel silver alloy that has excellent strength, stress relaxation resistance, and solderability. Due to it being extremely resistant to corrosion it doesn't tarnish easily and has a long s.. |
|||
Tensile Strength, Yield | 696 - 786 MPa | 101000 - 114000 psi | 0.2% offset |
Eagle Brass 770 Nickel Silver 18%, Extra Hard 770 has good cold forming properties, is tarnish resistant and has very good spring properties. 770 does not become subject to embrittlement at lower temperature and it has excellent corrosion resi.. |
|||
Tensile Strength, Yield | >= 696 MPa | >= 101000 psi | hardened to 300 HB |
Bohler-Uddeholm P20 PREMIUM MODIFIED Pre-hardened Mold Steel Cr-Mo alloyed steelP20 Modified offers the following benefits:No hardening risksNo hardening costsTime saving, e.g. no waiting for heat treatmentLower tool cost (e.g. no distortion to rectify)Modifi.. |