Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1005 MPa @Strain 0.200 %, Temperature 650 °C |
145800 psi @Strain 0.200 %, Temperature 1200 °F |
|
Haynes 242® alloy, cold reduced sheet, annealed, 40% cold work, aged Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
Tensile Strength, Yield | 1005 MPa @Strain 0.200 % |
145800 psi @Strain 0.200 % |
Typical |
TIMET 6-6-2 Titanium Alloy (Ti-6Al-6V-2Sn), Annealed Features: TIMETAL 6-6-2 offers improved strength properties and greater depth hardenability compared with TIMETAL 6-4.Data provided by TIMET. |