Polymer Property : Tensile Strength, Yield = 100.3 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 100.3 MPa
14550 psi
ASTM D638
Omni Plastics OmniTuff™ HPP GRC40 Homopolymer Polypropylene Glass Reinforced
Applications: Structural parts across industry segments including pump housings, wheels, handles, mountings, brackets, levers, pressure vessels, and furniture components.Information provided by Omni..