Polymer Property : Tensile Strength, Yield = 10.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 3.40 - 10.0 MPa
493 - 1450 psi
Average value: 8.00 MPa Grade Count:45
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Film Grade". Each property range of values reported is minimum a..