Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1.62 MPa | 235 psi | ASTM D412 |
Polymax® Maxelast® P2631 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Strength, Yield | 1.62 MPa | 235 psi | at 100% elongation, maximum |
Dow Corning SILASTIC® 25160 SILICONE RUBBER 60 durometer, peroxide cured, general purpose silicone rubber compoundInformation provided by Dow Corning |
|||
Tensile Strength, Yield | 1.62 MPa @Strain 300 % |
235 psi @Strain 300 % |
Method A (Dumbbell & Section), 20 in/min; ASTM D412 |
PolyOne Synprene® IT38-110 Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:High Performance Thermoplastic ElastomerNaturalTranslucentApplications:Multi-PurposeFDA (Food Contact)Market:Consumer GoodsProcessing Method:ExtrusionInjection MoldingPolyOne Fi.. |