Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1.33 MPa | 193 psi | AVG Stress at Elongation M25; ASTM D412 Method A |
Seals Eastern 5483 Nitrile Rubber Low temperature service NitrileInformation provided by Seals Eastern, Inc. |