Mechanical Properties Metric English Comments
Tensile Strength, Yield 1.21 MPa

@Strain 100 %
175 psi

@Strain 100 %
ASTM D412
Multibase Multi-Flex® A 4710 S Black TPE Thermoplastic Elastomer
Forms: PelletsProcessing Method:Injection Molding Information provided by Multibase