Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1.14 MPa | 165 psi | AVG Stress at Elongation M50; ASTM D412 Method A |
Seals Eastern 5722 Fluorocarbon-Elastomer Formulated Viton®. General service.Information provided by Seals Eastern, Inc. |