Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1.1000 MPa | 159.54 psi | at 150% elongation, maximum |
Dow Corning JCR 6122 Two-part, transparent, medium modulus LED encapsulant with very low viscosity, very long working time, and high transparency.Information provided by Dow Corning |