Polymer Property : Tensile Strength, Yield = 0.971 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 0.971 MPa
141 psi
ASTM D638
Cheng Yu Plastic E2325 Flame Retardant PET, 25% Glass Fiber
Tensile Strength, Yield 0.971 - 162 MPa
141 - 23500 psi
Average value: 118 MPa Grade Count:15
Overview of materials for Polyethylene Terephthalate (PET), 30% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 30% Glass Reinforced". Specific grades with glass content between 25% ..