Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 0.310 MPa @Strain 100 % |
45.0 psi @Strain 100 % |
ASTM D412 |
Multibase Multi-Flex® A 1540 Natural TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodSoftUV Resistance, Go.. |