Tensile Strength, Yield 0.0276 MPa
4.00 psi
4 PCF
Unifrax Insulfrax® S Blanket Insulation
Insulfrax S Blanket is a flexible, strong, lightweight, needled blanket produced from Insulfrax Fiber. Mechanical needling of the spun Insulfrax fibers eliminates the need for binders in the produc..
Tensile Strength, Yield 0.0276 MPa
4.00 psi
at 4 PCF; ASTM 686-76
Unifrax Fiberfrax® Durablanket® S Ceramic Fiber Insulator
Fiberfrax Durablanket S insulation is a strong, lightweight, flexible needled blanket that is made from spun ceramic fibers. Available in a wide variety of thicknesses, widths and densities, Durabl..