Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Falex Load Test 1.59e+6 g
3500 lb
EP Fail
ChevronTexaco Aries® 100
Texaco Aries lubricants deliver value through:Long equipment life — Extreme pressure performance withstands heavy shock loads typical of rock drill service, protecting the equipment against rapid w..
Falex Load Test 1.59e+6 g
3500 lb
EP Fail
ChevronTexaco Aries® 150
Texaco Aries lubricants deliver value through:Long equipment life — Extreme pressure performance withstands heavy shock loads typical of rock drill service, protecting the equipment against rapid w..
Falex Load Test 1.59e+6 g
3500 lb
EP Fail
ChevronTexaco Aries® 220
Texaco Aries lubricants deliver value through:Long equipment life — Extreme pressure performance withstands heavy shock loads typical of rock drill service, protecting the equipment against rapid w..
Falex Load Test 1.59e+6 g
3500 lb
EP Fail
ChevronTexaco Aries® 320
Texaco Aries lubricants deliver value through:Long equipment life — Extreme pressure performance withstands heavy shock loads typical of rock drill service, protecting the equipment against rapid w..
Falex Load Test 1.59e+6 g
3500 lb
ChevronTexaco Vistac® ISO 100 Rock Drill Oil
FeaturesChevron Rock Drill Oils Vistac are designed to give maximum protection to percussion rock drills.They are formulated from highly refined, high viscosity index, paraffinic base stocks and add..
Falex Load Test 1.59e+6 g
3500 lb
ChevronTexaco Vistac® ISO 32 Rock Drill Oil
FeaturesChevron Rock Drill Oils Vistac are designed to give maximum protection to percussion rock drills.They are formulated from highly refined, high viscosity index, paraffinic base stocks and add..
Falex Load Test 1.59e+6 g
3500 lb
ChevronTexaco Vistac® ISO 320 Rock Drill Oil
FeaturesChevron Rock Drill Oils Vistac are designed to give maximum protection to percussion rock drills.They are formulated from highly refined, high viscosity index, paraffinic base stocks and add..
Falex Load Test 1.59e+6 g
3500 lb
ChevronTexaco Vistac® ISO 46 Rock Drill Oil
FeaturesChevron Rock Drill Oils Vistac are designed to give maximum protection to percussion rock drills.They are formulated from highly refined, high viscosity index, paraffinic base stocks and add..
Falex Load Test 1.59e+6 g
3500 lb
EP Fail
ChevronTexaco Aries® 46
Texaco Aries lubricants deliver value through:Long equipment life — Extreme pressure performance withstands heavy shock loads typical of rock drill service, protecting the equipment against rapid w..
Falex Load Test 1.59e+6 g
3500 lb
ChevronTexaco Vistac® ISO 150 Rock Drill Oil
FeaturesChevron Rock Drill Oils Vistac are designed to give maximum protection to percussion rock drills.They are formulated from highly refined, high viscosity index, paraffinic base stocks and add..