Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Falex Load Test | 0.0160 g | 0.0000353 lb | Low Load, 600 lb for 2.5 hr |
ExxonMobil 100 Exxon Sawguide Oil EXXON SAWGUIDE OIL is specifically formulated to lubricate the thin saw blades of modern gang saws and edgers. The choice of viscosity grade depends on equipment type, lubricant delivery system desi.. |
|||
Falex Load Test | 0.0160 g | 0.0000353 lb | Low Load, 600 lb for 2.5 hr |
ExxonMobil 100 Exxon Sawguide Oil EXXON SAWGUIDE OIL is specifically formulated to lubricate the thin saw blades of modern gang saws and edgers. The choice of viscosity grade depends on equipment type, lubricant delivery system desi.. |