Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Timken Test | 36300 g | 80.0 lb | OK Load |
ChevronTexaco Pinnacle® EP 150 Texaco Pinnacle EP oils deliver value through:Excellent thermal and oxidation stability — The synthetic hydrocarbon base oils used in these products provide outstanding stability resulting in longe.. |
|||
Timken Test | 36300 g | 80.0 lb | OK Load |
ChevronTexaco Pinnacle® EP 220 Texaco Pinnacle EP oils deliver value through:Excellent thermal and oxidation stability — The synthetic hydrocarbon base oils used in these products provide outstanding stability resulting in longe.. |
|||
Timken Test | 36300 g | 80.0 lb | OK Load |
ChevronTexaco Pinnacle® EP 320 Texaco Pinnacle EP oils deliver value through:Excellent thermal and oxidation stability — The synthetic hydrocarbon base oils used in these products provide outstanding stability resulting in longe.. |
|||
Timken Test | 36300 g | 80.0 lb | OK Load |
ChevronTexaco Syn-Star® 320 Chain Oil Texaco Syn-Star Chain Oil 320 is a chain oil designed for use in extreme high and low temperature operations. It is formulated with synthetic base oils and an additive package which provides rust an.. |
|||
Timken Test | 36300 g | 80.0 lb | |
ChevronTexaco TEGRA® ISO 150 Synthetic Gear Lubricant FeaturesChevron Tegra Synthetic Gear Lubricants are superior quality industrial EP gear lubricants.The most advanced formulation has been selected to provide superior load carrying and antiwear prop.. |
|||
Timken Test | 36300 g | 80.0 lb | |
ChevronTexaco TEGRA® ISO 220 Synthetic Gear Lubricant FeaturesChevron Tegra Synthetic Gear Lubricants are superior quality industrial EP gear lubricants.The most advanced formulation has been selected to provide superior load carrying and antiwear prop.. |
|||
Timken Test | 36300 g | 80.0 lb | |
ChevronTexaco TEGRA® ISO 320 Synthetic Gear Lubricant FeaturesChevron Tegra Synthetic Gear Lubricants are superior quality industrial EP gear lubricants.The most advanced formulation has been selected to provide superior load carrying and antiwear prop.. |