Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Timken Test = 75.0 lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Timken Test 34000 g
75.0 lb
ASTM D-2596
ConocoPhillips Syncon® EP Heavy Duty Grease NLGI 1
Description: Conoco Syncon EP Heavy Duty Grease is an ultra high-performance synthetic base oil, lithium-complex grease specifically designed for extreme loading conditions. The combination of high-..
Timken Test 34000 g
75.0 lb
ASTM D-2596
ConocoPhillips Syncon® EP Heavy Duty Grease NLGI 2
Description: Conoco Syncon EP Heavy Duty Grease is an ultra high-performance synthetic base oil, lithium-complex grease specifically designed for extreme loading conditions. The combination of high-..
Timken Test 34000 g
75.0 lb
ConocoPhillips SynXPA® H-500 H Lubricant H-500
Description: Conoco SynXPA H Lubricant is a premium-quality synthetic-polyolester lubricant that offers protection for heavily loaded and partially opened open gears, such as those in ball mills, sh..
Timken Test 34000 g
75.0 lb
ConocoPhillips SynXPA® HC-450 H Lubricant HC-450
Description: Conoco SynXPA H Lubricant is a premium-quality synthetic-polyolester lubricant that offers protection for heavily loaded and partially opened open gears, such as those in ball mills, sh..
Timken Test 34000 g
75.0 lb
ChevronTexaco Delo® NLGI 2 Grease EP
FeaturesChevron Delo Greases EP are technically advanced, extreme pressure greases for a wide variety of on- and off-road applications.They are formulated with ISOSYN® base stocks, a lithium comple..
Timken Test 34000 g
75.0 lb
ChevronTexaco Delo® SAE 80W-90 Gear Lubricant ESI®
FeaturesChevron Delo Gear Lubricants ESI are premium grade, multipurpose gear lubricants.They are formulated with ISOSYN® base stocks and compounded with a unique extreme pressure additive utilizin..
Timken Test 34000 g
75.0 lb
ChevronTexaco Delo® SAE 85W-140 Gear Lubricant ESI®
FeaturesChevron Delo Gear Lubricants ESI are premium grade, multipurpose gear lubricants.They are formulated with ISOSYN® base stocks and compounded with a unique extreme pressure additive utilizin..
Timken Test 34000 g
75.0 lb
ChevronTexaco ISO 150 Ultra Gear Lubricant
FeaturesChevron Ultra Gear Lubricants are premium grade, multipurpose gear lubricants.They are formulated with a unique extreme pressure additive using an inorganic borate compound. ISO 68, 150, 220..
Timken Test 34000 g
75.0 lb
ChevronTexaco ISO 320 Ultra Gear Lubricant
FeaturesChevron Ultra Gear Lubricants are premium grade, multipurpose gear lubricants.They are formulated with a unique extreme pressure additive using an inorganic borate compound. ISO 68, 150, 220..
Timken Test 34000 g
75.0 lb
ChevronTexaco ISO 460 Ultra Gear Lubricant
FeaturesChevron Ultra Gear Lubricants are premium grade, multipurpose gear lubricants.They are formulated with a unique extreme pressure additive using an inorganic borate compound. ISO 68, 150, 220..
Timken Test 34000 g
75.0 lb
ChevronTexaco ISO 680 Ultra Gear Lubricant
FeaturesChevron Ultra Gear Lubricants are premium grade, multipurpose gear lubricants.They are formulated with a unique extreme pressure additive using an inorganic borate compound. ISO 68, 150, 220..
Timken Test 34000 g
75.0 lb
ConocoPhillips Centak Centak 11 Extreme Pressure Gear Lubricant
Description: Conoco Centak is a high-quality, multipurpose, extreme-pressure gear lubricant recommended for the open gears of shovels and draglines. It may also be used in grinding mills, swing gear..
Timken Test 34000 g
75.0 lb
ConocoPhillips IGL-9 Enclosed Gear Lubricant ISO 1000, AGMA Number 8A EP
Description: Conoco IGL-9 Enclosed Gear Lubricant is a superior-quality, black, heavy, extreme-pressure gear lubricant developed specifically for enclosed gear sets operating under severe service co..
Timken Test 34000 g
75.0 lb
ConocoPhillips IGL-9 Enclosed Gear Lubricant ISO 460, AGMA Number 7EP
Description: Conoco IGL-9 Enclosed Gear Lubricant is a superior-quality, black, heavy, extreme-pressure gear lubricant developed specifically for enclosed gear sets operating under severe service co..
Timken Test 34000 g
75.0 lb
ConocoPhillips IGL-9 Enclosed Gear Lubricant ISO 680, AGMA Number 8EP
Description: Conoco IGL-9 Enclosed Gear Lubricant is a superior-quality, black, heavy, extreme-pressure gear lubricant developed specifically for enclosed gear sets operating under severe service co..
Timken Test 34000 g
75.0 lb
ChevronTexaco ISO 220 Ultra Gear Lubricant
FeaturesChevron Ultra Gear Lubricants are premium grade, multipurpose gear lubricants.They are formulated with a unique extreme pressure additive using an inorganic borate compound. ISO 68, 150, 220..