Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Timken Test | 38500 g | 85.0 lb | OK Load |
ChevronTexaco Pinnacle® EP 1000 Texaco Pinnacle EP oils deliver value through:Excellent thermal and oxidation stability — The synthetic hydrocarbon base oils used in these products provide outstanding stability resulting in longe.. |
|||
Timken Test | 38500 g | 85.0 lb | OK Load |
ChevronTexaco Pinnacle® EP 460 Texaco Pinnacle EP oils deliver value through:Excellent thermal and oxidation stability — The synthetic hydrocarbon base oils used in these products provide outstanding stability resulting in longe.. |
|||
Timken Test | 38500 g | 85.0 lb | |
ChevronTexaco TEGRA® ISO 460 Synthetic Gear Lubricant FeaturesChevron Tegra Synthetic Gear Lubricants are superior quality industrial EP gear lubricants.The most advanced formulation has been selected to provide superior load carrying and antiwear prop.. |
|||
Timken Test | 38500 g | 85.0 lb | |
ChevronTexaco TEGRA® ISO 680 Synthetic Gear Lubricant FeaturesChevron Tegra Synthetic Gear Lubricants are superior quality industrial EP gear lubricants.The most advanced formulation has been selected to provide superior load carrying and antiwear prop.. |
|||
Timken Test | 38500 g | 85.0 lb | OK Load |
ChevronTexaco Pinnacle® EP 680 Texaco Pinnacle EP oils deliver value through:Excellent thermal and oxidation stability — The synthetic hydrocarbon base oils used in these products provide outstanding stability resulting in longe.. |