Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Timken Test | 15900 g | 35.0 lb | |
ConocoPhillips 1 HD Calcium Grease NLGI No. 1 Description: Conoco HD Calcium Grease is a formulated product, ideally suited for equipment exposed to corrosive fluids, saltwater or extremely high temperatures. HD Calcium Grease is used exclusive.. |
|||
Timken Test | 15900 g | 35.0 lb | |
ConocoPhillips 2 HD Calcium Grease NLGI No. 2 Description: Conoco HD Calcium Grease is a formulated product, ideally suited for equipment exposed to corrosive fluids, saltwater or extremely high temperatures. HD Calcium Grease is used exclusive.. |
|||
Timken Test | 15900 g | 35.0 lb | |
ConocoPhillips 2 Bentone Grease NLGI No. 2 Description: Conoco Bentone Grease is a high-quality, smooth-textured, clay based grease developed for heavy-duty industrial machinery operating at very high temperatures. Unlike conventional soap-b.. |