Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 63.6 - 68.9 MPa
9220 - 9990 psi
3M 6146 Kraft Medium Duty Reinforced Water Activated Tape
3M™ Medium Duty Reinforced Water Activated Tape 6146 Kraft is used for box sealing and other packaging applications. This product has a fiberglass reinforced paper backing and high tack water activ..