Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 41.4 - 62.1 MPa | 6000 - 9000 psi | ASTM D882 |
Honeywell ACLAR® 11A (3.00 mil) CTFE Homopolymer, Barrier Film
(discontinued **) Description: ACLAR® 11A is a CTFE homopolymer, high performance barrier film for industrial and electronics applications.Information provided by Honeywell. |
|||
Film Tensile Strength at Break, MD | 41.4 - 62.1 MPa | 6000 - 9000 psi | ASTM D882 |
Honeywell ACLAR® 11A (2.00 mil) CTFE Homopolymer, Barrier Film
(discontinued **) Description: ACLAR® 11A is a CTFE homopolymer, high performance barrier film for industrial and electronics applications.Information provided by Honeywell. |
|||
Film Tensile Strength at Break, MD | 41.4 - 62.1 MPa | 6000 - 9000 psi | ASTM D882 |
Honeywell ACLAR® UltRx 3000 CTFE Homopolymer, Barrier Film Description: ACLAR® UltRx 3000 is a 3 mil CTFE homopolymer high performance barrier film for the pharmaceutical and medical markets. It thermoforms well on conventional blister packaging equipme.. |