Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD >= 89.6 MPa
>= 13000 psi
ASTM D882
DuPont™ Tedlar® TTR10BG3 Transparent Polyvinyl Fluoride Film
Properties of DuPont™ Tedlar® polyvinyl fluoride (PVF) biaxially oriented film include excellent resistance to weathering, outstanding mechanical properties, and inertness towards a wide variety o..
Film Tensile Strength at Break, MD >= 89.6 MPa
>= 13000 psi
ASTM D882
DuPont™ Tedlar® TUT10BG3 UV Screening Transparent Polyvinyl Fluoride Film
Properties of DuPont™ Tedlar® polyvinyl fluoride (PVF) biaxially oriented film include excellent resistance to weathering, outstanding mechanical properties, and inertness towards a wide variety o..
Film Tensile Strength at Break, MD 89.6 MPa
13000 psi
20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
ExxonMobil Label-Lyte™ 70LS447 OPP Film
Product Description: A two-side coated, shrink resistant, white, polypropylene film designed for use in hot melt cut-and stack labeling. It has an static resistant, matte finish, paper like print su..
Film Tensile Strength at Break, MD 89.6 MPa
13000 psi
ASTM D882
Dow SARAN WRAP™ 3 Plastic Film
SARAN WRAP™ 3 Plastic Film is a clear biaxially oriented monolayer barrier film, designed for tight wrap and heat sealing applications. It is available in 50 gauge, as single or double would rolls..
Film Tensile Strength at Break, MD 89.6 MPa
13000 psi
ASTM D882
ExxonMobil Exceed™ 3518CB Metallocene Polyethylene Resin (European Grade)
Product Description: Exceed 3518CB is a metallocene ethylene-hexene copolymer. Films made of Exceed 3518CB grade have outstanding tensile, impact and puncture resistance properties. Furthermore, the..