Polymer Property : Film Tensile Strength at Break, MD = 8850 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 28.3 - 61.0 MPa
4100 - 8850 psi
Average value: 46.2 MPa Grade Count:34
Overview of materials for Linear Low Density Polyethylene (LLDPE)/Octene, Film