Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | >= 87.0 MPa | >= 12600 psi | 400 N/10mm |
Dr. D. Mueller Flexiso® DMD FI 14010 00460 Polyester Electrical Insulation Structure: Flexiso® DMD, FI 14010 00460 is a flexible three layer material, consisting of a layer of polyester film, of which both sides have a layer of polyester fleece fabric and is coated with .. |