Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 58.75 MPa | 8521 psi | ASTM D882 |
Dow TUFLIN™ HS-7066 NT 7 Linear Low Density Polyethylene Resin Hexene Linear Low Density Resin Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a TUFLIN™ HS-7066 NT 7 is a fractional melt, ethylene-hexene copolymer, designed for good toughness and stiffness. Th.. |