Polymer Property : Film Tensile Strength at Break, MD = 8130 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 56.1 MPa
8130 psi
ASTM D882
Dow FLEXOMER™ ETS-9066 NT 7, 2mil Very Low Density Polyethylene (VLDPE) Resin
FLEXOMER™ ETS-9066 NT 7 is intended for use in single of multi-layer blown-film constructions or thick sheets. Films extruded from ETS-9064 NT 7 have a high tear strength, high impact strength, an..