Polymer Property : Film Tensile Strength at Break, MD = 8000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 41.4 - 55.2 MPa
6000 - 8000 psi
ASTM D882
Honeywell ACLAR® 22C (5.00 mil) Copolymer Film  (discontinued **)
Description: ACLAR® 22C is a copolymer film consisting primarily of chlorotrifluoroethylene (CTFE). It has moisture barrier and is used for electroluminescent lamps.Information provided by Honeywe..