Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 35.0 - 54.0 MPa
5080 - 7830 psi
Average value: 43.0 MPa Grade Count:3
Overview of materials for High Density Polyethylene (HDPE), Copolymer Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Copolymer Film Grade". Each property range of values reported is minim..