Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 51.5 MPa | 7470 psi | ASTM D882 |
Chevron Phillips Dynex™ D605A6 Enhanced LLDPE Blown Film Resin