Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 25.5 - 74.5 MPa | 3700 - 10800 psi | Average value: 44.0 MPa Grade Count:80 |
Overview of materials for Linear Low Density Polyethylene (LLDPE)/Hexene, Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE)/Hexene, Film Grade". Each property range of values reported is m.. |